Blasted. Then zink primer and 2 coats stone chip. Done.
T t400ble Junior Member Messages 39 Apr 11, 2019 #61 Blasted. Then zink primer and 2 coats stone chip. Done.
T t400ble Junior Member Messages 39 Apr 12, 2019 #63 Stone chip is great but you need to deal with the issues underneath first
T t400ble Junior Member Messages 39 Apr 12, 2019 #64 Attachments IMG-20190412-WA0019.jpeg 819.6 KB · Views: 7
T t400ble Junior Member Messages 39 Apr 12, 2019 #65 Subframe time now where the pipe overs fit Terrible water trap. Cup wire brush in the grinder soon cleans then up and then rust treatment then a zink coat then stone chip. Bloody car.
Subframe time now where the pipe overs fit Terrible water trap. Cup wire brush in the grinder soon cleans then up and then rust treatment then a zink coat then stone chip. Bloody car.